![]() Fig. 01: Test block with water supply. |
![]() Fig. 02: Test block with water supply. |
![]() Fig. 03: Ladle containing molten metal (grey cast iron, approx. 1450°C) |
![]() Fig. 04: Pouring into the wet test block with a continuous water supply. |
![]() Fig. 05: Pouring into the wet test block with a continuous water supply. |
![]() Fig. 06: The water pours over the molten metal. |
![]() Fig. 07: A cross-section of the cast. |